3M 1099L

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

3M 1099L

Main features

  • Approximately 40-Minute Open Time
  • Spray, Brush, or Roller Application
  • Water, Oil, and Fuel Resistance

Product Description

3M Nitrile High Performance Plastic Adhesive 1099L is a lower-viscosity, solvent-based nitrile adhesive for flexible bonds to most vinyls and plastics, excluding polyolefins. Its approximately 40-minute open time provides an interval for joining coated surfaces after spray, brush, or roller application. The adhesive dries at room temperature; optional heat curing can increase bond strength. Finished bonds resist weathering, water, oil, fuels, and plasticizer migration. This combination of coating options, assembly time, and flexible bond behavior suits vinyl upholstery, automotive panel installation, banners, and awnings.

Key features

  • Approximately 40-minute open time: Coated surfaces can be positioned and joined within this assembly window.
  • Spray, brush, or roller application: The lower-viscosity grade can be coated with industrial spray equipment or applied manually.
  • Fluid and plasticizer resistance: Finished bonds resist water, oil, fuels, plasticizer migration, and weathering.

Applications

Bonding most vinyls and plastics except polyolefins; aftermarket automotive panel installation and upholstery; banners and awnings; general industrial and MRO bonding.

Product Family

3M 1099L

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
Light Tan
SolidsSolids
22-26 %
Thermal Properties
Flash PointFlash Point
-18 °C
Physical Properties
ViscosityViscosity
200-325 mPa.s
Other Properties
Storage TemperatureStorage Temperature
16 - 27 °C

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers