3M 1280

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

3M 1280

Main features

  • 3.6 mil Polyester Tape
  • 33.9 N/100 mm Steel Adhesion
  • Low-Stretch PCB Masking

Product Description

3M Circuit Plating Tape 1280 is a red polyester-film masking tape with a silicone/rubber adhesive for printed circuit board electroplating, solder stripping, and precious-metal finger masking. Its typical 3.6 mil total thickness includes a 0.9 mil backing. The low-stretch film helps control stop-off lines, while the thick adhesive coating reduces plating-solution undercutting between circuit fingers. Typical adhesion to steel is 33.9 N/100 mm by ASTM D3330, and the maximum operating temperature is 155 deg C. The tape can be applied by hand or machine with firm pressure to establish contact.

Key features

  • 3.6 mil total construction: A 0.9 mil polyester backing is combined with a silicone/rubber adhesive coating; thicknesses are typical ASTM D3652 values.
  • 33.9 N/100 mm steel adhesion: Typical adhesion is measured by ASTM D3330 on steel.
  • Plating-process temperature limit: Maximum operating temperature for the tape is 155 deg C.

Applications

Printed circuit board masking during solder stripping and precious-metal finger plating; splicing silicone-treated papers.

Product Family

3M 1280

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
Red
Total ThicknessTotal Thickness
91 μm
Mechanical Properties
ElongationElongation
135 %
Tensile Strength (Thin Film)Tensile Strength (Thin Film)
52.54 N/cm
Other Properties
Storage TemperatureStorage Temperature
15 - 27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Values are typical and not specifications.

PropertyValueUnitMethod / condition
BackingPolyester film-Red tape construction
AdhesiveSilicone/rubber blend-Pressure-sensitive coating
Backing thickness0.9milASTM D3652
Total tape thickness3.6milASTM D3652
Standard roll length72 or 144ydAvailable roll lengths
Technical properties

After-processing / final-state properties

Values are typical and not specifications.

PropertyValueUnitMethod / condition
Adhesion to steel33.9N/100 mmASTM D3330
Tensile strength at break525.4N/100 mmASTM D3759
Elongation at break135%ASTM D3759
Maximum operating temperature155deg CApplied tape

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers