3M 2290

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M 2290

Main features

  • Approximately 21% Solids Coating
  • Up to Three-Month B-Stage Window
  • Multiple Metal-Coating Methods

Product Description

3M Scotch-Weld Epoxy Adhesive 2290 is a one-part, solvent-based thermosetting epoxy adhesive and coating for metal bonding and lamination. The amber-tinted, low-viscosity formulation contains approximately 21% solids and can be brushed, sprayed, or applied by flow, dip, roll, or knife coating. Solvent removal produces a tack-free B-staged film, allowing coated parts to be stored for up to three months before final heat-cured bonding. Heat pressing is recommended for lamination. Supported uses include motor stator and rotor laminations, copper foil bonding to B-staged epoxy in printed circuits, coils, and thin metal stacks.

Key features

  • Approximately 21% solids: The solvent-based epoxy is applied as a low-viscosity coating before solvent removal and heat cure.
  • Delayed final bonding: Tack-free B-staged coated parts can be stored for up to three months before final heat curing.
  • Six coating methods: Brush, flow, dip, roll, knife, and spray application accommodate different coating processes.

Applications

Electric-motor stator and rotor laminations; copper foil bonding to B-staged epoxy in printed circuits; coils and electronic subassemblies; thin metal stack laminations.

Product Family

3M 2290

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
Light Amber
Density (g)Density (g)
0.86-0.91 g/cm3
SolidsSolids
19.5-23 %
Thermal Properties
Flash PointFlash Point
-14 °C
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
95 °C
Physical Properties
ViscosityViscosity
40-80 mPa.s
Other Properties
Storage TemperatureStorage Temperature
16 - 27 °C
Electrical Properties
Volume ResistivityVolume Resistivity
1.2 x 10¹⁵ Ohms⋅cm

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers