3M 5354
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Main features
- Non-Curing Butyl Sealant Tape
- Low Moisture-Vapor Transmission
- Vertical, Overhead, and Corner Placement
Product Description
3M Weatherban Sealant Tape 5354 is a permanently tacky, non-curing butyl sealant tape for joints between glass, metal, wood, EPDM rubber, and many plastics. The black, 100% solids synthetic-rubber extrusion compresses into the interface and adheres to clean, dry surfaces. Typical water-vapor transmission is 0.39 g/m2 per 24 hours by ASTM E96-66 Procedure B. The tape resists cold flow and stays in place on vertical or overhead surfaces and around sharp corners. It should be aligned carefully as it comes off the roll, because repositioning usually distorts the sealant rather than allowing clean relocation.
Key features
- Non-curing sealant construction: The 100% solids synthetic-rubber tape remains tacky and requires no mixing or cure schedule.
- Water-vapor transmission: The typical material value is 0.39 g/m2 per 24 hours by ASTM E96-66 Procedure B.
- Vertical and overhead placement: The high-tack extrusion stays positioned on dry surfaces and around sharp corners.
Applications
Sealing between glass, metal, wood, EPDM rubber, and many plastics.