3M 590

Main features

  • 25 to 40-Minute Tack-Free Time
  • Polycarbonate and Acrylic Bonding
  • FMVSS 212 Crash Tested

Product Description

3M Polyurethane Glass Adhesive Sealant 590 is a one-component, moisture-curing polyurethane paste for bonding glass, acrylic/PMMA, and polycarbonate windows in vehicle and marine assemblies. It requires no mixing and is applied between 5 and 35 deg C, with primer recommended for window bonding. Typical tack-free time is 25 to 40 minutes at 73 deg F and 50% relative humidity; cure progresses at more than 3.5 mm per 24 hours under those conditions. The cured adhesive has typical tensile strength of 10 MPa by ASTM D412 and Shore A hardness 60 to 65 by ASTM C661.

Key features

  • Moisture-cure processing: Typical tack-free time is 25 to 40 minutes at 73 deg F and 50% RH; this is separate from through-thickness cure.
  • 10 MPa tensile strength: Typical cured-material tensile strength is measured by ASTM D412; Shore A hardness is 60 to 65 by ASTM C661.
  • Primed window bonding: Primer is recommended when bonding glass or plastic windows with this one-component polyurethane.

Applications

Structural windshield installations; PMMA windshields; polycarbonate and acrylic bonding; flush-mounted marine and automotive glass.

Product Family

3M 590

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Physical Properties
Tack-Free TimeTack-Free Time
25 - 40 minutes
Mechanical Properties
ElongationElongation
>700 %
General Properties
Specific GravitySpecific Gravity
1.2
Other Properties
Storage TemperatureStorage Temperature
Below 25 °C

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers