3M 730

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

3M 730

Main features

  • Clear Isocyanate-Free SMP
  • 40 to 60-Minute Skin Time
  • Paintable While Wet

Product Description

3M Sealant 730 UV is a clear, one-component silane-modified polymer sealant for cosmetic panel joints in vehicles and architectural assemblies. The isocyanate-free, low-VOC formulation cures with moisture, fills joint gaps, and remains permanently elastic after cure. A surface skin forms in 40 to 60 minutes while moisture curing continues within the joint. Water-based paint can be applied while the sealant is wet. Its transparent appearance and UV resistance suit exposed seams where a visible opaque sealant line is undesirable, including panel sealing on trucks, trains, trailers, and specialty vehicles.

Key features

  • Clear SMP sealant: The one-component, isocyanate-free formulation forms a transparent, permanently elastic joint seal.
  • 40 to 60-minute skin time: This interval applies to formation of the surface skin, not full cure.
  • Wet-paint compatibility: Water-based paint can be applied before the sealant has dried or cured.

Applications

Panel sealing on trucks, trains, trailers, and specialty vehicles; architectural panels.

Product Family

3M 730

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Physical Properties
Tack-Free TimeTack-Free Time
25 - 30 minutes
Mechanical Properties
ElongationElongation
300 %
General Properties
Specific GravitySpecific Gravity
1.05
Other Properties
Storage TemperatureStorage Temperature
Below 25 °C

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers