Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M LSB60NS

Main features

  • 90-Minute Work Life
  • 1:1 Epoxy Mixing
  • 3,500 psi Aluminum Overlap Shear

Product Description

3M Scotch-Weld Toughened Epoxy Adhesive LSB60NS is a gray, non-sag two-part toughened epoxy for meter-mix dispensing and large-panel structural bonding. Base and accelerator mix 1:1 by volume and weight. Typical open time is 90 minutes before bond closure. At 23 deg C, typical work life is 90 minutes, handling time to 0.3 MPa overlap shear is five hours, and full cure takes seven days. Component viscosities are typically 24,000 cP for the base and 97,000 cP for the accelerator at 27 deg C by Brookfield RTV. The cured adhesive has typical Shore D hardness 62 and 3,500 psi overlap shear on prepared aluminum after seven days at 23 deg C.

Key features

  • 90-minute work life: The typical static-mixer work life applies at 23 deg C; maximum open time before bond closure and fixing is also 90 minutes.
  • Equal-ratio meter-mix processing: The base-to-accelerator ratio is 1:1 by both volume and weight.
  • 3,500 psi aluminum overlap shear: Typical strength applies to prepared aluminum after seven days at 23 deg C.

Applications

Delivery-truck side walls; metal-enclosure facing and cabinets; panels to frame.

Product Family

3M LSB60NS

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Gray
Component SystemComponent System
Two (Accelerator | Base)
Physical Properties
Open timeOpen time
90 minutes
Other Properties
Storage TemperatureStorage Temperature
16 - 27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Values are typical and not specifications.

PropertyValueUnitMethod / condition
Mix ratio by volume (B:A)1:1-Two-part system
Mix ratio by weight (B:A)1:1-Two-part system
Base viscosity24,000cP27 deg C; Brookfield RTV
Accelerator viscosity97,000cP27 deg C; Brookfield RTV
Open time90minMaximum before bond closure and fixing
Work life90min23 deg C; static mixing nozzle
Time to handling strength5h23 deg C; time to 0.3 MPa overlap shear
Time to full cure7d23 deg C

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers