3M PTFE 5490
Harmonization Code : 8529.90 | Parts solely or principally used for TV, radio, and transmission

Main features
- Low-Friction Non-Stick Surface
- Flat Extruded PTFE Backing
- Clean-Removal Silicone Adhesive
Product Description
3M PTFE Film Tape 5490 has been discontinued. It is an adhesive-backed extruded PTFE film tape with a silicone pressure-sensitive adhesive. The 0.05 mm PTFE backing creates a smooth, low-friction, non-stick surface, while the 0.09 mm total tape construction lies flat and resists curling during unwind. The tape supports web movement, release, masking, and temporary chemical-barrier functions on process surfaces. Its silicone adhesive provides clean removal from a range of substrates. Commercial organic solvents can attack the adhesive, so solvent exposure is an important selection limit for the intended application.
Key features
- Low-friction non-stick surface: Supports web movement and clean release on rollers, plates, belts, and other process equipment.
- Flat curl-resistant backing: The extruded PTFE film lies flatter than typical skived PTFE tape and resists curling during unwind.
- Clean-removal silicone adhesive: Provides pressure-sensitive attachment and clean removal from a range of compatible surfaces.
Applications
Applications include low-friction web handling on rollers and formers, easy-release surfaces on rollers, plates, and belts, temporary sealing and masking, and machinery noise or rattle reduction.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Mechanical Properties
Other Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Color | Brown | As supplied | |
| Adhesive type | Silicone | Pressure-sensitive adhesive | |
| Backing | Extruded PTFE | Polytetrafluoroethylene | |
| Backing thickness | 0.05 | mm | ASTM D3652 |
| Total tape thickness | 0.09 | mm | ASTM D3652 |
After-processing / final-state properties
Performance values are typical for the tape construction; long-term temperature values refer to exposure over days or weeks.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| 180 deg peel adhesion | 2.9 | N/cm | ASTM D3330; 22 deg C; 300 mm/min |
| Elongation at break | 170 | % | ASTM D3759 |
| Tensile strength | 30.4 | N/cm | ASTM D3759 |
| Maximum long-term temperature resistance | 260 | deg C | Typical; days to weeks |
| Minimum long-term temperature resistance | -54 | deg C | Typical; days to weeks |