3M TE040

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M TE040

Main features

  • 2-Minute Open Time
  • 40-Second Handling Strength
  • 7,000 cP Warm-Application Viscosity

Product Description

3M Scotch-Weld PUR Adhesive TE040 is a one-component, 100% solids reactive polyurethane hot-melt adhesive supplied as a black extrudable solid. Typical viscosity is 7,000 cP at 121 deg C by Brookfield Thermosel, and typical open time is two minutes for a 3.2 mm bead on a nonmetallic surface. After bond formation, typical handling time is 40 seconds to support a 5 psi tensile load. Moisture curing subsequently develops the urethane bond, with typical cured Shore D hardness 35. The adhesive bonds wood, fiber-reinforced plastics, other plastics, metal, and glass for furniture, cabinetry, profile wrapping, and panel assembly.

Key features

  • 7,000 cP application viscosity: The typical value for the black grade is measured at 121 deg C by Brookfield Thermosel.
  • 40-second handling time: This typical minimum interval is the time for the bond to support a 5 psi tensile load, not full moisture cure.
  • Reactive one-component PUR: The 100% solids hot melt combines initial handling strength with subsequent moisture-curing urethane bond development.

Applications

Wood or plastic bonding for furniture and cabinetry; profile wrapping for windows and doors; panel assembly.

Product Family

3M TE040

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
White/Off-White
Density (g)Density (g)
1.07 g/cm3
Physical Properties
Open timeOpen time
2 minutes
ViscosityViscosity
7,000 mPa.s
Mechanical Properties
ElongationElongation
860 %
Other Properties
Storage TemperatureStorage Temperature
Below 49 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Values are typical and not specifications.

PropertyValueUnitMethod / condition
Component countOne-Reactive PUR hot melt
FormExtrudable solid-Black grade
Solids content100%As supplied
Viscosity7,000cP121 deg C; Brookfield Thermosel
Open time2min3.2 mm bead on a non-metallic surface
Time to handling strength40sTime to support a 5 psi tensile load

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers