ABchimie LDM High-Temperature Solder Mask

Harmonization Code : 32159090 | Printing ink, writing or drawing ink, and other inks, whether or not concentrated or solid, specifically for those classified as other within that category

ABchimie LDM High-Temperature Solder Mask

Main features

  • Dries at room temperature
  • Withstands temperatures up to 270°C
  • Can be completely removed by hand

Product Description

ABchimie LDM is a flexible, low‑viscosity copolymer‑based compound designed to protect precise areas of printed circuit boards during various manufacturing processes. It forms a reliable temporary mask that withstands production steps such as coating, assembly, and wave soldering. LDM requires clean, oil‑free, grease‑free, and silicone‑free surfaces for optimal adhesion, and is fully compliant with REACH and RoHS regulations.

Produt Key Features

  • Can be completely removed by hand without leaving residue
  • Insoluble in solvents and does not contaminate conformal coatings or varnishes
  • Forms a tough, tear‑resistant protective film
  • Withstands temperatures up to 270°C for several seconds (maximum 8 seconds), suitable for wave soldering exposure

Applications

Product Family

ABCHIMIE LDM

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
EU Shipping in 8 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
White liquid
Density (g)Density (g)
1 g/cm3
Mechanical Properties
ElongationElongation
900 %

Additional Information

Instructions for Use

To apply LDM on the part to protect, by soaking, brushing or with the beak of the supple bottle in polyethylene. LDM contains ammonia. It should be used in a well-ventilated room.

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers