LOCTITE ABLESTIK 563K

Harmonization Code : 3920.99.28.90 | Other plates, sheets, film, foil and strip, of plastics, non-cellular and not reinforced, laminated, supported or similarly combined with other materials ; Of other plastics ; Other; Other

LOCTITE ABLESTIK 563K

Main features

  • Good heat transfer
  • Low squeeze out
  • Thermally conductive

Product Description

LOCTITE ABLESTIK 563K epoxy adhesive film is suitable for bonding "hot" devices onto heat sinks where electrical insulation and good heat transfer are required. It exhibits low squeeze out during bonding. This product provides high strength over a wider temperature range than is normally associated with flexible films.

LOCTITE ABLESTIK 563K  is a thermally conductive film with good heat transfer which manages to achieve a thin bondline with uniform bondline control. It comes without a carrier and is typically available in 50um and 75um microns.

 

Cure Schedule

  • 30 minutes @ 150°C
  • 2 hours @ 125°C
Product Family

ABLESTIK 563K

1. Select Package Type
2. Select Thickness
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 20 days
CA Shipping in 12 weeks
EU Shipping in 45 days
Packaging
Please select Package Type and Thickness.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Work life @25°CWork life @25°C
2160 hours
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
97 °C
Thermal ConductivityThermal Conductivity
1.1 W/m.K

Additional Information

Outgassing

NASA Outgassing:

  • TML, % 0.44
  • CVCM, % 0.04
  • WVR, % 0.2

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers