LOCTITE ABLESTIK 8-2

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE ABLESTIK 8-2

Main features

  • Thermally conductive
  • Positive under UV light
  • For MEMs packages

Product Description

LOCTITE ABLESTIK 8-2 non-conductive die attach adhesive is designed for MEMs package applications. Designed as an instrument adhesive, LOCTITE ABLESTIK 8-2 adhesive offers eight times the thermal conductivity of unfilled epoxies. Bonds made with LOCTITE ABLESTIK 8-2 can withstand continuous exposure @ 150 °C and intermittent exposure @ 200°C.

Cure Schedule

  • 1.5hours @ 95ºC
  • 45 minutes @ 120°C or
  • 4 hours @ 75°C or
  • 24 hours @ 60°C
Product Family

ABLESTIK 8-2

1. Select Package Type
2. Select Package Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 30 days
CA Shipping in 12 weeks
EU Shipping in 50 days
Packaging
Please select Package Type and Package Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific GravitySpecific Gravity
2.3
Work life @25°CWork life @25°C
4 hours
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
92 °C
Thermal ConductivityThermal Conductivity
1.5 W/m.K
Weight Loss @ 300°CWeight Loss @ 300°C
0.1 %

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers