LOCTITE ABLESTIK 8175

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE ABLESTIK 8175

Main features

  • Stress absorbing
  • Pb free Solder replacement
  • Stencil or Screen printable

Product Description

LOCTITE ABLESTIK 8175 is designed for solder replacement in microelectronic interconnect applications. This adhesive may be used with thick film metallizations or traditional printed circuit board surfaces. It is capable of resolving fine pitch resolution (0.02 inch) when printed using either a stainless steel mesh screen or a metal mask stencil.

LOCTITE ABLESTIK 8175 meets the requirements of MIL-STD-883, Method 5011. It is a stress absorbing, electrically and thermally conductive epoxy adhesive that is typically used for die attach. This is a stencil and screen printable Pbfree alternative to solder.

Cure Schedule

  • 30 minutes @ 150°C
  • 60 minutes @ 150°C (for bondlines lower than 1mil)
  • 60 minutes @ 130°C
Product Family

ABLESTIK 8175

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 21 days
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Work life @25°CWork life @25°C
336 hours
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
90 °C
Thermal ConductivityThermal Conductivity
3.2 W/m.K
Weight Loss @ 300°CWeight Loss @ 300°C
0.3 %
Electrical Properties
Volume ResistivityVolume Resistivity
0.0005 Ohms⋅cm
Physical Properties
Thixotropic indexThixotropic index
2
ViscosityViscosity
55,000 mPa.s

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers