LOCTITE ABLESTIK 8200T

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE ABLESTIK 8200T

Main features

  • High electrical conductivity
  • Snap curable
  • Excellent adhesion to Ag plated LF

Product Description

LOCTITE ABLESTIK 8200T electrically conductive die attach adhesive is designed for high reliability package applications with medium thermal and electrical requirements. This material offers improved JEDEC performance on QFN type packages.

LOCTITE ABLESTIK 8200T is hybrid silver adhesive that is snap curable and has excellent adhesion to Ag plated leadframe. It is typically used on PPF and Silver substrates and exhibits very low bleed.

Cure Schedule

  • 30 minute ramp to 175°C + 15 minutes @ 175°C
Product Family

ABLESTIK 8200T

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Work life @25°CWork life @25°C
24 hours
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
241 °C
Thermal ConductivityThermal Conductivity
2.5 W/m.K
Electrical Properties
Volume ResistivityVolume Resistivity
0.0001 Ohms⋅cm
Chemical Properties
Moisture absorptionMoisture absorption
0.3 %
Physical Properties
ViscosityViscosity
9,000 mPa.s

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers