LOCTITE ABLESTIK E 8502-1

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE ABLESTIK E 8502-1

Main features

  • One component
  • Low stress
  • Thermally conductive

Product Description

LOCTITE ABLESTIK E 8502-1 is a solventless modified epoxy non-conductive adhesive known for its versatility in bonding applications. LOCTITE ABLESTIK E 8502-1 boasts a formulation that combines low-stress properties with strong adhesion capabilities across a wide array of surfaces.

LOCTITE ABLESTIK E 8502-1 flexibility makes it well-suited for scenarios involving disparate coefficients of thermal expansion (CTE), ensuring effective bonding even in mismatched CTE situations. 

Product Family

ABLESTIK E8502-1

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 20 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific GravitySpecific Gravity
1.15 - 1.2
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
60 - 70 °C
Thermal ConductivityThermal Conductivity
0,6 W/m.K
Electrical Properties
Surface ResistivitySurface Resistivity
170000000000000 Ohms/sq
Volume ResistivityVolume Resistivity
40700000000000 Ohms⋅cm
Physical Properties
ViscosityViscosity
40000 - 50000 mPa.s

Additional Information

Curing schedule

Temperature Cure time
120°C 90
150°C 60
175°C 15

 

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers