LOCTITE ABLESTIK ICP 8311

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE ABLESTIK ICP 8311

Main features

  • Snap curable
  • Sn Compatible
  • Jet Dispensing & Stenci printing

Product Description

LOCTITE® ABLESTIK ICP 8311 is an electrically conductive adhesive designed for applications where a fast cure is required. It is ideally suited for high throughput photovoltaic dispense and print processes and applications where high adhesion strength is required. Low and stable contact resistance is achieved on substrates containing Sn during reliability testing.

LOCTITE® ABLESTIK ICP 8311 is a flexible acrylate that is compatible with Sn (Tin). It is typically used for flexible interconnects in photovoltaic shingle applications. It is developed for solar panel applications with max 25um filler cut and DSC onset temperature of 60° Celsius, suitable for high volume jet dispensing, screen printing and stencil printing processes.

Cure Schedule

  • 10 - 15 seconds @ 150°C
Product Family

ABLESTIK ICP8311

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 41 days
CA Shipping in 12 weeks
EU Shipping in 30 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

Electrical Properties
Volume ResistivityVolume Resistivity
0.00039 Ohms⋅cm
Physical Properties
Thixotropic indexThixotropic index
4.2
ViscosityViscosity
14,600 mPa.s

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers