LOCTITE ABLESTIK QMI505MT

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE ABLESTIK QMI505MT

Main features

  • Electrically conductive
  • Low modulus
  • Skip Cure

Product Description

LOCTITE® ABLESTIK QMI505MT die attach paste is designed for attachment of integrated circuits and components to advanced metal and ceramic surfaces. A package or device manufactured with LOCTITE ABLESTIK QMI505MT will have good resistance to delamination and “popcorning” after exposure to reflow temperatures.

LOCTITE® ABLESTIK QMI505MT is a hydrophobic, electrically conductive rubberized epoxy with low modulus that reduces inter package stress. This silver filled adhesive has excellent interfacial adhesion strength and is stable at high temperatures. Typically used for SBGA, OFN and TQFP packages and on gold, silver, ceramic, palladium and alloy42 surface finishes.

Skip Cure

  • ≥10 seconds @ 200°C
Product Family

ABLESTIK QMI505MT

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Pot LifePot Life
48 hours
Specific GravitySpecific Gravity
3.42
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
-10 °C
Thermal ConductivityThermal Conductivity
2.4 W/m.K
Electrical Properties
Volume ResistivityVolume Resistivity
0.002 Ohms⋅cm
Chemical Properties
Moisture absorptionMoisture absorption
0.2 %
Physical Properties
Thixotropic indexThixotropic index
4.8
ViscosityViscosity
12,000 mPa.s

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers