ALPHA EF-2100

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

ALPHA EF-2100

Main features

  • 4.0 wt% Solids Content
  • ORL0 No-Clean Flux
  • Lead-Free Hole-Fill Performance

Product Description

ALPHA EF-2100 is a VOC-free, halide-free, rosin/resin-free, low-solids no-clean liquid flux for wave soldering and through-hole assembly. Its 4.0 wt% solids formulation is classified ORL0 under IPC J-STD-004 and has less than 1% VOC content. Typical processing uses 95 to 115 deg C top-side preheat and 2 to 7 seconds of solder contact time. In lead-free assemblies, it provides good hole fill with low solder balling and bridging and leaves an evenly spread, tack-free residue.

Key features

  • 4.0 wt% low-solids formulation: The 4.0 wt% solids level is paired with less than 1% VOC content in the as-supplied liquid flux.
  • Lead-free hole-fill performance: The flux provides good hole fill with low solder balling and bridging in lead-free assemblies.
  • IPC flux classification: J-STD-004 designation is ORL0 for the halide-free, rosin/resin-free no-clean formulation.

Applications

Wave soldering and through-hole assembly for lead-free soldering, including applications requiring good hole fill and low solder balling or bridging.

Product Family

ALPHA EF-2100

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Clear, colorless liquid
Specific GravitySpecific Gravity
1.015±0.003
Physical Properties
VOCVOC
<1

Additional Information

Technical properties

As supplied

PropertyValueUnitMethod / condition
Solids content4.0wt%Typical
Specific gravity1.015 +/- 0.003Typical at 25 deg C
pH2.2Typical; as is
Acid number31.5 +/- 2.0mg KOH/gTypical
VOC content<1%Typical
Shelf life18monthsTypical
IPC J-STD-004 designationORL0As supplied

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers