ALPHA EF-6103 is a low-solids, alcohol-based no-clean liquid flux for wave and selective soldering. Typical as-supplied data include 3.6 wt% solids, specific gravity of 0.796 +/- 0.004 at 25 deg C, a 360-day shelf life, and IPC J-STD-004B classification ORL0. It can be applied by spray or foam. Typical processing uses 95 to 125 deg C top-side preheat, 2 to 7.5 seconds of lead-free wave solder contact, and 2 to 5 seconds for selective soldering.

Key features

  • Dual soldering process fit: The flux is applied in both wave and selective soldering processes.
  • IPC flux classification: J-STD-004B designation is ORL0.
  • 360-day shelf life: This is the typical storage period for the as-supplied liquid flux.

Applications

Wave soldering and selective soldering using spray or foam flux application.

Product Family

ALPHA EF-6103

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Clear, light amber liquid
Specific GravitySpecific Gravity
0.796±0.004
Thermal Properties
Flash PointFlash Point
12 °C

Additional Information

Technical properties

As supplied

PropertyValueUnitMethod / condition
Solids content3.6wt%Typical
Specific gravity0.796 +/- 0.004Typical at 25 deg C
Acid value22.4 +/- 1.3mg KOH/gTypical
Flash point12deg CT.C.C.
Shelf life360daysTypical
IPC J-STD-004B classificationORL0As supplied
Technical properties

Uncleaned test coupons

PropertyValueUnitMethod / condition
Surface insulation resistance - comb-down6.6 x 10^9ohmTest result; IPC J-STD-004A; uncleaned; 85 deg C/85% RH for 7 days; -50 V bias, 100 V measurement on IPC B-24
Surface insulation resistance - comb-up2.1 x 10^10ohmTest result; IPC J-STD-004A; uncleaned; 85 deg C/85% RH for 7 days; -50 V bias, 100 V measurement on IPC B-24
Bellcore surface insulation resistance - comb-down1.7 x 10^11ohmTest result; GR-78-CORE Issue 1; uncleaned; 35 deg C/85% RH for 4 days; 48 V bias, 100 V measurement; 25 mil lines/50 mil spacing
Bellcore surface insulation resistance - comb-up2.1 x 10^11ohmTest result; GR-78-CORE Issue 1; uncleaned; 35 deg C/85% RH for 4 days; 48 V bias, 100 V measurement; 25 mil lines/50 mil spacing

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers