ALPHA OM-535

Harmonization Code : 3810.10.00 | Soldering, brazing or welding powders and pastes consisting of metal and other materials

ALPHA OM-535

Main features

  • Enables elimination of a second or third reflow cycle
  • 8+ Hour stencil life
  • Compatible with all commonly used Pb-free surface finishes

Product Description

ALPHA OM-535 features a low-temperature solder paste technology that enables a single reflow application for the assemby of double-sided boards. It has excellent no-solder drip phenomena during the reflow process. ALPHA OM-535 with SBX02 alloy has been successfuly used with peak reflow profiles between 155 - 190℃. This version also shows a higher mechanical strength and drop shock resistance than SnBi0.4Ag alloy. The flux in ALPHA OM-535 has excellent electrical resistivity than exceeds industry standards.

ALPHA OM-535 enables the elimination of an extra wave or selective wave soldering process when temperature sensitive through-hole components are used in an assembly.

Product Key Features

  • Increased daily throughput, eliminating the need for managing wave solder.
  • Removes the need for an extra SMT process, which significantly lower the cost of producing an electronic assembly.
  • The alloys yield very low voiding BGA solder joints, even when a traditional  SAC alloy sphere is used.

Applications

  • Assembly of double-sided boards requiring a single reflow application.
  • Applications demanding low-temperature soldering and reflow profiles between 155 - 190℃
Product Family

ALPHA OM-535

1. Select Alloy Type
2. Select Package Type
3. Select Particle Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
Shipping in 3 weeks
Packaging
Please select Alloy Type, Package Type and Particle Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Alloy TypeAlloy Type
SBX02, SnBi0.4Ag, 42Sn57Bi1Ag

Additional Information

OM-535 Reflow Profile

Reflow Profile

Application

  • STENCIL: Recommend ALPHA CUT, ALPHA NICKEL-CUT, ALPHA TETRABOND®, or ALPHA FORM stencils @ 0.100 mm - 0.150 mm (4-6 mil) thick for 0.4 - 0.5 mm (0.016” or 0.020”) pitch. Stencil design is subject to many process variables. Contact your local Alpha stencil site for advice. 
  • SQUEEGEE: Metal recommended 
  • PRESSURE: 0.21 - 0.36 kg/cm of blade (1.25 -2.0 Ibs/inch) 
  • SPEED: 25 – 100 mm per second (1 – 6 inches per second) 
  • PASTE ROLL: 1.5-2.0 cm diameter and make additions when roll reaches 1 cm (0.4”) diameter (min). Max roll size will depend upon blade. 
  • STENCIL RELEASE SPEED: 1 – 5 mm/sec 
  • LIFT HEIGHT: 8 – 14 mm(0.31 – 0.55”)

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers