ALPHA PV-50
Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

Main features
- Low-Solids Alcohol-Based Flux
- Zero-Halogen No-Clean Chemistry
- Low/No-Preheat Tabbing Process
Product Description
ALPHA PV-50 is a low-solids, alcohol-based no-clean liquid flux for tabbing and stringing photovoltaic cells during solar-module assembly. The formulation is zero-halogen, halide-free, and rosin-free. It is applied in low- or no-preheat tabbing and stringing processes, with standard soldering following the fluxing step.
Key features
- Halogen and resin profile: The no-clean formulation is zero-halogen, halide-free, and rosin-free.
- Low/no-preheat processing: Tabbing and stringing can use low or no preheat before standard soldering.
- Photovoltaic assembly use: The flux is applied during solar-module tabbing and stringing operations.
Applications
Solar module assembly tabbing and stringing using low or no preheat followed by standard soldering.