ALPHA SM-110 Solvent Cleaner
Harmonization Code : 29051200 | Propan-1-ol (propyl alcohol) and propan-2-ol (isopropyl alcohol)

Main features
- High solvency
- High flux loading capacity
- Non-corrosive
Product Description
ALPHA SM‑110 Cleaner is a high‑performance blend of organic solvents engineered for fast, efficient, non‑aqueous cleaning in electronics manufacturing. Formulated to deliver superior cleaning strength with low odor and zero water rinse requirements, ALPHA SM‑110 provides a reliable and cost‑effective solution for modern SMT production environments.
Designed as areplacement for IPA, ALPHA SM‑110 evaporates rapidly and leaves no residue, making it an ideal choice for operations seeking improved productivity, safer handling, and enhanced performance across a wide range of cleaning tasks.
Product Key Features
- Effective cleaner at ambient temperature
- Ideal for stencil cleaning and non-aqueous batch cleaning
- High solvency of solder paste residues.
- High flux loading capacity
Applications
- Removing solder paste from stencils.
- Post-soldering flux residue removal from electronic assemblies
Packaging
Technical Specifications
General Properties
Thermal Properties
Physical Properties
Additional Information
Application
| Application | Description |
| Stencil Cleaning | Removes Raw Solder Paste, Removes Uncured SMT Adhesives |
| Finger Cleaning | Fluxes Used in Wave Soldering |
| Pallet Cleaning | Fluxes Used in Wave Soldering |
| Bench Top/Rework Cleaning | Removes Flux Residues |
| Post-Soldering Cleaning | Removes Flux Residues (Wave Solder & Reflow) |
| General-Purpose Cleaning | Equipment / Area Clean-Up |
| Conformal Coating Removal | Removes Most Silicone & Acrylic Conformal Coatings (Cured & Uncured) |