ARALDITE CY8043

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

ARALDITE CY8043

Main features

  • 23 to 26% Bromine Content
  • 3,000 to 4,000 cP at 25 deg C
  • Flame-Retardant Casting Formulation Resin

Product Description

ARALDITE CY 8043 is a brominated epoxy resin for flame-retardant electrical and electronic casting formulations. It is a yellow-to-light-brown resin with approximately 3,000 to 4,000 cP viscosity at 25 deg C, 23 to 26% bromine, and 0.42 to 0.46 eq/100 g epoxy content. Flash point is approximately 185 deg C. Applications include filament winding, casting and encapsulation, wet lay-up laminates, and adhesive formulations where this brominated epoxy resin is used as a formulation component.

Key features

  • 23 to 26% bromine content: The exact grade contains 23 to 26% bromine.
  • 3,000 to 4,000 cP viscosity: As-supplied viscosity is approximately 3,000 to 4,000 cP at 25 deg C.
  • 0.42 to 0.46 eq/100 g epoxy content: Epoxy content is 0.42 to 0.46 eq/100 g.

Applications

Filament winding, casting and encapsulation, wet lay-up laminates, and adhesive formulations.

Product Family

ARALDITE CY8043

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Yellow to light brown
Physical Properties
ViscosityViscosity
@ 25°C, 3000 - 4000 mPa.s
Thermal Properties
Flash PointFlash Point
>185 °C

Additional Information

Technical properties

As supplied

PropertyValueUnitMethod / condition
AppearanceYellow to light brownAs supplied
ViscosityApprox. 3,000 to 4,000cP25 deg C
Bromine content23 to 26%As supplied
Epoxy content0.42 to 0.46eq/100 gAs supplied
Flash pointApprox. 185deg CAs supplied

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers