ARALDITE LT8049

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

ARALDITE LT8049

Main features

  • 47 to 50% Bromine Content
  • 322 to 357 g/eq Epoxy Equivalent
  • White Crystalline Powder or Flakes

Product Description

ARALDITE LT 8049 is a solid brominated epoxy resin supplied as white powder or flakes for flame-retardant epoxy formulations. Specified epoxy index is 2.80 to 3.10 eq/kg, epoxy equivalent is 322 to 357 g/eq, bromine content is 47 to 50%, and hydrolyzable chlorine is no more than 300 ppm. Typical melting point is 105 to 115 deg C. The crystalline resin is used in flame-retarded printed circuit board formulations and in powder-coating or molding-powder formulations.

Key features

  • 47 to 50% bromine content: Specified bromine content is 47 to 50%.
  • 322 to 357 g/eq epoxy equivalent: Specified epoxy equivalent is 322 to 357 g/eq.
  • White crystalline powder or flakes: The solid resin is supplied as white powder or flakes for formulation handling.

Applications

Flame-retarded printed circuit board formulations and flame-retardant powder-coating or molding-powder formulations.

Product Family

ARALDITE LT8049

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
White flakes
DensityDensity
@25ºC, ∼ 1.8 kg/m3
Chemical Properties
Melting PointMelting Point
105°C - 115°C
Thermal Properties
Flash PointFlash Point
200 °C

Additional Information

Technical properties

As supplied

PropertyValueUnitMethod / condition
AppearanceWhite powder / flakesSpecified
Epoxy index2.80 to 3.10eq/kgSpecified
Epoxy equivalent322 to 357g/eqSpecified
Bromine content47 to 50%Specified
Hydrolyzable chlorine<= 300ppmSpecified
Melting point105 to 115deg CTypical
DensityApprox. 1.8g/cm^3Typical; 25 deg C
Flash point>= 200deg CTypical

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers