AXAREL 56
Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

Main features
- Water-Rinsible Heavy-Soil Cleaning
- Heated-Immersion Process Fit
- Buffing-Compound and Grease Removal
Product Description
AXAREL 56 Solvent Cleaner uses highly refined solvents and surfactants in a water-rinsible formulation for heated immersion processing. It targets difficult soils that demand elevated-temperature cleaning, including buffing compounds, heavy greases, and other high-melting residues. The solvent-and-surfactant system combines strong soil removal with a water-rinse process step, making it relevant to precision-cleaning operations where residue removal follows heated soak treatment. Its supported uses include commercial and general aviation cleaning, precision cleaning, and heated immersion cleaning.
Key features
- Water-rinsible formulation: Refined solvents and surfactants fit cleaning processes that include a water rinse.
- Heated immersion use: Formulated for elevated-temperature soak cleaning.
- Heavy-soil removal: Targets buffing compounds, heavy greases, and high-melting residues.
Applications
Applications include commercial and general aviation cleaning, precision cleaning, and heated immersion cleaning.