AXAREL 850
Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

Main features
- Low-Concentration Inline Defluxing
- 1 mil Standoff Residue Removal
- Non-Foaming Additive-Free Operation
Product Description
AXAREL 850 Low Concentration Inline Defluxer is an inherently non-foaming aqueous cleaner for spray-in-air inline systems. Used at 3 to 5% concentration, it improves removal of water-soluble flux residue beneath components with standoff heights as low as 1 mil. The formulation offers high flux-loading capacity and requires no anti-foaming agents or other additives to maintain the cleaning approach. Recommended wash-bath temperatures are 120 to 160 deg F (50 to 70 deg C), followed by a 150 deg F (65 deg C) DI-water rinse. It is intended for low-concentration defluxing of electronic assemblies.
Key features
- 3 to 5% inline cleaning: Low working concentration fits aqueous spray-in-air systems.
- Low-standoff residue removal: Improves water-soluble flux removal under component gaps as low as 1 mil.
- Inherently non-foaming: Requires no anti-foaming agents or other additives.
Applications
Applications include low-concentration aqueous inline defluxing to remove water-soluble flux residue from electronic assemblies.
TDS, SDS & Technical Documents
Technical Specifications
Thermal Properties
General Properties
Physical Properties
Additional Information
As-supplied / before-processing properties
Typical product properties and recommended wash and rinse conditions.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Odor | Mild | - | Typical |
| Flash point | None to boiling | - | Typical |
| Specific gravity | 0.955 | - | 25 deg C; typical |
| pH | 10.2 | - | 5% concentration; typical |
| Viscosity | 12 | cps | Typical |
| Wash-bath concentration | 3 to 5 | % | Recommended process range |
| Wash-bath temperature | 120 to 160 (50 to 70) | deg F (deg C) | Recommended process range |
| DI-water rinse temperature | 150 (65) | deg F (deg C) | Recommended |