BOSTIK 915
Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other

Main features
- 35% Dynamic Joint Movement
- 685% Cured Elongation
- 60-Minute Tooling Window
Product Description
Bostik 915 is a one-component, moisture-curing polyurethane sealant and adhesive for joint sealing and bonding applications. It cures to a tough, flexible rubber with +/-35% dynamic joint movement capability and 685% elongation after the documented cure condition, supporting joints that require substantial movement accommodation. A 60-minute tool/work time provides a practical installation window before skin formation, while cured performance is listed from -40 to 150 deg F. The product is used for expansion and control joints, door and window perimeters, wall penetrations, roofing details, metal roofs, gutters, roof tiles, flashing, and sheet-metal sealing within the manufacturer's construction scope.
Key features
- 35% Dynamic Joint Movement: Demonstrates +/-35% joint movement capability under the documented movement test.
- 685% Cured Elongation: Provides 685% elongation at break after the documented 14-day cure condition.
- 60-Minute Tooling Window: A 60-minute tool/work time supports joint placement and finishing.
Applications
Expansion and control joints; door and window perimeters; wall penetrations; roofing, metal roofs, gutters, roof tiles, flashing, and sheet-metal sealing within the documented construction scope.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Mechanical Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Tool / work time | 60 | min | Typical |
| Skin time | 4 | hours | Typical |
| Cure time | 2 to 7 | days | 77 deg F; varies with relative humidity |
| Flow / sag / slump | 0.3 | in | Typical |
| Shelf life | 1 | year | Unopened cartridge; store at 10 to 32 deg C |
Final-state properties
Typical cured properties after 14 days at 77 deg F and 50% RH unless otherwise noted.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Hardness | 42 | Shore A | ASTM D2240 |
| Modulus at 100% | 65 | psi | ASTM D412 |
| Tensile strength at break | 133 | psi | ASTM D412 |
| Elongation at break | 685 | % | ASTM D412 |
| Adhesion peel | Greater than 5 | piw | TT-S-00230C / ASTM C794 |
| Joint movement capability | +/-35 | % | TT-S-00230C / ASTM C719 |
| UV resistance | Pass | ASTM C793 | |
| Service temperature | -40 to 150 | deg F | Cured service range |