BOSTIK PE103

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BOSTIK PE103

Main features

  • 100% Solids Web Adhesive
  • Moderate 105 deg C Activation
  • Uniform Fine-Filament Adhesive Coverage

Product Description

Bostik PE103 is a nonwoven polyester hot-melt web adhesive supplied in roll form for flexible laminating. The fine-filament web handles like a fabric and works in intermittent or continuous processes, with basis-weight options from 15 to 100 g/yd^2. Dry heat activation requires 105 deg C, and reactivation time depends on process conditions. PE103 bonds fabrics, foams, and vinyls and is used in automotive interior, door-trim, and carpeting laminations as well as footwear and apparel bonding.

Key features

  • 100% solids web: Nonwoven polyester web is a 100% solids adhesive format.
  • Moderate heat activation: Dry heat activation requires 105 deg C.
  • Uniform adhesive coverage: Fine-filament web provides uniform coverage for intermittent or continuous processing.

Applications

Automotive interior, door-trim, and carpeting laminations plus footwear and apparel bonding.

Product Family

BOSTIK PE103

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Milky White
Basis WeightBasis Weight
18-120 g/m2
WidthWidth
25 - 173 cm
Chemical Properties
Melting PointMelting Point
103

Additional Information

Technical properties

As-supplied properties

PropertyValueUnitMethod / condition
AppearanceMilky whiteTypical physical property
Basis weight range15 to 100g/yd^2Typical physical property
Trimmed width10 to 68inTypical roll width
Melt point103deg CTypical physical property
Solids content100%Product format
Shelf life24monthsStored below 54 deg C

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers