CONAP CE-1170

Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other

CONAP CE-1170

Main features

  • One-Component Acrylic Conformal Coating
  • 15-Minute Tack-Free Time
  • 2 x 10^15 ohm-cm Volume Resistivity

Product Description

CONAP® CE-1170 Acrylic Conformal Coating is a one-component, solvent-based acrylic conformal coating for printed circuit boards, epoxy-glass laminates, phenolic laminates, components, and other thin-film electronic applications. The coating is room-temperature or heat curable, with a typical tack-free time of 15 minutes, full cure in 24 hours at 25°C, or accelerated cure in 45 minutes at 60°C. It is documented as flexible, quick drying, repairable, humidity resistant, and hydrolytically stable, with a typical volume resistivity of 2 × 10¹⁵ ohm·cm.

Key features

  • One-component acrylic coating: The solvent-based material is used for thin-film protection of components and printed circuitry.
  • Fast handling: Typical tack-free time is 15 minutes, with room-temperature or accelerated heat cure.
  • Electrical insulation: Typical volume resistivity is 2 × 10¹⁵ ohm·cm.

Applications / Suitable for

  • Printed circuit boards and printed circuitry
  • Epoxy-glass and phenolic laminates
  • Thin-film coating of electronic components
Product Family

CONAP CE-1170

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Physical Properties
ViscosityViscosity
400 mPa.s
VOCVOC
5.5 lb/gal
General Properties
AppearanceAppearance
Amber, slight haze
Specific GravitySpecific Gravity
0.95
Thermal Properties
Flash PointFlash Point
13 °C
Electrical Properties
Dielectric StrengthDielectric Strength
>118.11 kV/mm
Volume ResistivityVolume Resistivity
2 x 10¹⁵ Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or mixed-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Chemical base Acrylic N/A One-component solvent-based coating
Color Amber N/A One-gallon can configuration
Specific gravity 0.93 N/A As supplied
Viscosity 400 cP As supplied
Tack-free time 15 min Typical
Cure options 24 h at 25°C; 45 min at 60°C N/A Room-temperature or heat cure
Flash point 7 °C One-gallon can configuration

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers