CONATHANE MR-5016
Harmonization Code : 3215907090 | Ink, whether or not concentrated or solid (excl. printing ink, printer/copier ink cartridges incorporating mechanical or electrical components, and solid ink in engineered shapes for printers/copiers)

Main features
- Low-Viscosity Mold Release Application
- 100% Solids Silicone System
- 12-Month Shelf Life
Product Description
CONAP MR-5016 Mold Release Agent is a low-viscosity silicone-polymer liquid release and parting agent for potting, casting, and molding operations. The clear, 100% solids material has an approximate viscosity of 225 cP at 25 deg C and specific gravity of approximately 0.97. Its flash point is above 201 deg F, and the product has a 12-month shelf life under the stated storage conditions. Applications include release of epoxy, polyurethane, polyester, and other plastic or resin systems from non-porous molds, including simple and complex mold geometries.
Key features
- Low-viscosity release: Approximate viscosity is 225 cP at 25 deg C for liquid mold-release application.
- 100% solids silicone system: Clear silicone-polymer material with approximately 0.97 specific gravity.
- 12-month shelf life: Shelf life is 12 months under the stated storage conditions.
Applications
Mold release for epoxy, polyurethane, polyester, and other plastic or resin systems from non-porous molds.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Thermal Properties
Additional Information
As-supplied properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Clear | As supplied | |
| Viscosity | Approx. 225 | cP | 25 deg C |
| Specific gravity | Approx. 0.97 | 25 deg C | |
| Solids | 100 | % | As supplied |
| Flash point | Above 201 | deg F | As supplied |
| Shelf life | 12 | months | Stated storage conditions |