COOLTHERM 6716

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

COOLTHERM 6716

Main features

  • 45-Minute Mixed Working Window
  • 100:2.5 Resin-Hardener Ratio
  • Low- and High-Voltage Encapsulation

Product Description

Circalok 6716 Silicone Resin is the resin component of a two-component, solvent-free RTV silicone system used with Circalok 6733 hardener. The black liquid has a typical viscosity of 10,000 cP and specific gravity of 1.40 at 25 deg C. When combined with Circalok 6733 hardener, the resin and hardener mix at 100:2.5 by weight, provide a typical 45-minute working life at 25 deg C, and cure in 12 to 16 hours at 25 deg C. The system is used for potting and encapsulating both low- and high-voltage electrical and electronic assemblies.

Key features

  • 6733 Hardener Pairing: Circalok 6716 resin is formulated for use with Circalok 6733 hardener.
  • 45-Minute Working Life: The 6716/6733 mixed system has a typical 45-minute working life at 25 deg C.
  • Electrical Assembly Encapsulation: The 6716/6733 system is used for potting low- and high-voltage electrical and electronic assemblies.

Applications

Resin component for the Circalok 6716/6733 silicone system used to pot and encapsulate low- and high-voltage electrical and electronic assemblies.

Product Family

COOLTHERM 6716

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Black Liquid
Specific GravitySpecific Gravity
1.40
Physical Properties
ViscosityViscosity
10,000 mPa.s
Electrical Properties
Volume ResistivityVolume Resistivity
1 x 10^15 Ohms⋅cm
Thermal Properties
Thermal ConductivityThermal Conductivity
0.3 W/m.K
Mechanical Properties
ElongationElongation
200 %

Additional Information

Technical properties

As-Supplied Properties

Values apply to the Circalok 6716 resin component as supplied.

PropertyValueUnitMethod / condition
AppearanceBlack liquidTypical; 6716 resin
Viscosity10,000cPTypical; 6716 resin; 25 deg C
Specific gravity1.40Typical; 6716 resin; 25 deg C

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers