BMI-6000 Imide-extended Bismaleimide Oligomer
Harmonization Code : 2925.19.95.90 | Carboxyimide-function compounds (including saccharin and its salts) and imine-function compounds : Imides and their derivatives; salts thereof : Other : Other : Other

Main features
- Superior thermal stability
- Good dielectric properties
- Toughener
Product Description
BMI-6000 has been designed as a curable, low DK and Df alternative to replace both the Kapton and adhesive layers in the manufacture of FCCL materials. The material has excellent thermal stability and workability. It is soluble in a variety of solvents such as cyclopentanone, cyclohexanone, MEK, DMF, DMAC, and NMP in combination with aromatic solvents. It can be processed in a resin system as a solid or dissolved in a solvent.
BMI-6000 is recommended for use as an adhesive layer when laminating materials for FCCL applications. Adhesion promoters, solvent(s), are required for successful use. BMI6000 has much higher Tg than products such as BMI-689 and require thermal curing to obtain the published values. This material is not suitable for UV curing.
Aromatic BMI resins lose some of their user-friendly nature compared to the aliphatic versions: they are less soluble in normal solvents, less compatible with other resins, require more complicated curing processes, etc.
Packaging
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Additional Information
What are the main differences with BMI 6100?
- The reaction to form the product is performed in anisole and for economy, we prefer to leave it in anisole
- We are unable to precipitate this higher molecular weight material to form a solid powder - it forms a gooey mess.