MM290| Acrylate adhesion promoter Additive
Harmonization Code : 2916.12 | Unsaturated acyclic monocarboxylic acids and their anhydrides, halides, peroxides, peroxyacids, and their derivatives

Main features
- Mild pleasant odor
- Hydrolytic resistance
- Lower weight loss on cure than IBOA
Product Description
MM-290 is a liquid mono-functional acrylate monomer. It has similar properties as Isobornyl Acrylate (IBOA) when polymerized but with lower weight loss on cure. It has a mild, pleasant odor. MM-290 has good resistance to hydrolysis.
MM-290 is recommended for use in UV or peroxide cure formulations. It is particularly recommended for applications that require hydrolytic resistance. This monomer has a much, much, much better smell than isobornyl acrylates and has a significantly lower weight loss.
Packaging
Please select Package Type.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
AppearanceAppearance
Light tan liquidDensity (g)Density (g)
0.98 g/cm3Thermal Properties
Flash PointFlash Point
175 °CPhysical Properties
ViscosityViscosity
110 mPa.s