PEAM-1044 Low warpage Polyester Acrylate/Methacrylate

Harmonization Code : 3906909090 | Acrylic polymers in primary form Others>Others

PEAM-1044 Low warpage Polyester Acrylate/Methacrylate

Main features

  • Thermally stable
  • Low warpage
  • High adhesion to various substrates

Product Description

PEAM-1044 is a polyester acrylate/methacrylate that exhibits excellent adhesion, low warpage, and hydrophobicity. The oligomer has very high thermal stability and low volatility. It can be used as a base resin in a formulation or an additive. It is dark amber-colored, something that needs to be considered for light cure application.

PEAM-1044 is recommended for use as a base resin. It has excellent adhesion with low stress due to its high Tg DCPD units. The oligomer has good solubility in both aliphatic and aromatic resins. Exceptionally low warpage can be achieved with the addition of polybutadiene type resins. Compared to what most people use (epoxies) the PEAM-1044 is composed of large, low functionality, oligomers instead of small, highly cross-linked monomers. That's why it is common to use PEAM 645 which is more akin to epoxies or a combination of both.

Product Family

DMI PEAM-1044

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US No longer available
CA No longer available
EU Shipping in 2 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Amber Liquid
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
-25 °C
Weight Loss @ 300°CWeight Loss @ 300°C
3 %
Physical Properties
ViscosityViscosity
4,500 mPa.s

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers