DOWSIL 7094

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

DOWSIL 7094

Main features

  • Self-Leveling Flowable Placement
  • 400% Cured Elongation
  • 25-Minute Skin-Over Time

Product Description

DOWSIL 7094 Flowable Sealant flows and self-levels into gaps where a one-part, neutral-cure silicone sealant is required for sealing or bonding. The black or white viscous liquid has a typical density of 1.30 g/cm^3 and viscosity of 28,000 mPa s, allowing flow into gaps and airless-spray application. At 23 deg C and 50% relative humidity, it skins in about 25 minutes, becomes tack-free in about 50 minutes and cures inward from the exposed surface. After seven days under those conditions, the sealant has Shore A 19 hardness, 400% elongation and 1.2 MPa tensile strength.

Key features

  • Flowable self-leveling rheology: Typical viscosity is 28,000 mPa s for gap filling and spray application.
  • 25-minute skin-over time: Supports tooling and assembly before surface cure.
  • Flexible cured seal: Typical elongation is 400% with Shore A 19 hardness.

Applications

Sealing and bonding applications requiring a low-viscosity, self-leveling silicone sealant.

Product Family

DOWSIL 7094

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Black or white, viscous liquid
Density (g)Density (g)
1.30 g/cm3
Physical Properties
ViscosityViscosity
28,000 mPa.s
Mechanical Properties
ElongationElongation
400 %

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied and cure-development properties. Values are not specifications.

Property Value Unit Method / condition
Appearance Black or white viscous liquid As supplied
Density 1.30 g/cm^3 CTM0097B
Viscosity 28000 mPa s CTM0050
Skin-over time 25 min CTM0098; 23 deg C and 50% RH
Tack-free time 50 min CTM0095A; 23 deg C and 50% RH
Cure depth About 2 mm After 24 hr at room temperature and 50% RH
Shelf life 12 months Below 30 deg C in original unopened container
Technical properties

After-processing / final-state properties

Typical mechanical properties after seven days in air at 23 deg C and 50% relative humidity.

Property Value Unit Method / condition
Tensile strength 1.2 MPa CTM0137A
Elongation at break 400 % CTM0137A
Modulus at 100% 0.36 MPa CTM0137A
Hardness 19 Shore A CTM0099

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers