DOWSIL 734

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

DOWSIL 734

Main features

  • Self-Leveling Flowable Placement
  • 7-Minute Tack-Free Time
  • 17 kV/mm Dielectric Strength

Product Description

DOWSIL™ 734 Flowable Sealant is a one-part, moisture-curing acetoxy silicone adhesive sealant supplied as a flowable, self-leveling liquid. It is used for general industrial sealing and bonding where the material must flow into fine joints, cracks, crevices, cable entries, connectors, and other difficult-to-fill interfaces. The sealant skins over in approximately 7 minutes and becomes tack-free in approximately 13 minutes at room temperature. After cure, it forms a tough, flexible silicone rubber with a typical Shore A hardness of 27, 315% elongation at break, dielectric strength of 17 kV/mm, and flexibility across a documented temperature range of -65°C to 180°C. Its adhesion to existing silicone rubber also makes it suitable for field repair of previously encapsulated equipment.

Key features

  • Flowable, self-leveling consistency: The 45,000 mPa·s liquid can flow into fine joints, voids, cracks, crevices, and narrow assembly interfaces.
  • One-part moisture cure: The acetoxy silicone cures at room temperature when exposed to atmospheric moisture without component mixing.
  • Fast surface-cure development: Typical skin-over and tack-free times are approximately 7 and 13 minutes, respectively.
  • Flexible cured silicone rubber: Typical cured properties include Shore A 27 hardness, 1.5 MPa tensile strength, and 315% elongation at break.
  • Electrical insulation properties: Typical dielectric strength is 17 kV/mm with volume resistivity of 1 × 1015 Ω·cm after the specified cure.
  • Wide documented temperature range: The cured material remains stable and flexible from -65°C to 180°C.

Applications / Suitable for

  • General industrial sealing and bonding requiring a flowable material
  • Fine joints, cracks, crevices, and narrow assembly interfaces
  • Cable entries and electrical or electronic connectors
  • Field repair of equipment containing existing silicone encapsulants
Product Family

DOWSIL 734

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Flowable liquid
ColorColor
Clear, white
Specific GravitySpecific Gravity
1.03
Physical Properties
Tack-Free TimeTack-Free Time
13 minutes
ViscosityViscosity
45,000 mPa.s
Electrical Properties
Dielectric StrengthDielectric Strength
17 kV/mm
Volume ResistivityVolume Resistivity
1E15 Ohms⋅cm

Additional Information

Industrial silicone sealant

DOWSIL™ 734 Flowable Sealant

DOWSIL™ 734 Flowable Sealant is a one-part acetoxy silicone adhesive sealant that flows and self-levels into fine joints, cracks, crevices, cable entries, and connector interfaces. It cures through exposure to atmospheric moisture and forms a tough, flexible rubber with useful mechanical and electrical insulation properties.

One-part acetoxy silicone Flowable and self-leveling 45,000 mPa·s viscosity 7-minute skin-over time Clear or white
DOWSIL™ 734 Flowable Sealant product packaging

DOWSIL™ 734 Flowable Sealant is available in clear and white.

As supplied

Flow and surface-cure characteristics

Viscosity
45,000 mPa·s
Typical value at 25°C. The flowable consistency supports penetration into narrow joints and irregular voids.
Skin-over time
7 minutes
Typical surface-skin formation at room temperature and 50% relative humidity. Tooling should be completed before the skin forms.
Tack-free time
13 minutes
Typical tack-free development is distinct from complete through-cure and should not be treated as service readiness.
Property Typical value Unit Method / condition
Appearance Flowable liquid — CTM 0176
Available colors Clear, white — As supplied
Viscosity at 25°C 45,000 mPa·s CTM 0050 / ASTM D1084
Skin-over time 7 minutes CTM 0098
Tack-free time 13 minutes CTM 0095
Non-volatile content 95 % CTM 0208; after 24 hours at 70°C

Typical values are not intended for use as product specifications.

Processing

Application and cure guidance

The sealant cures from the exposed surface inward through reaction with moisture in the air. Surface preparation, applied thickness, atmospheric moisture access, and cure time should therefore be considered when evaluating the material for an assembly.

Surface preparation: Surfaces must be clean and dry. Remove contaminants that could impair adhesion using a suitable solvent such as isopropyl alcohol, acetone, or methyl ethyl ketone.
Application thickness: Apply a uniform layer approximately 0.25 to 0.75 mm thick. For bonding, apply to one surface and use sufficient assembly pressure to spread the sealant and displace trapped air.
Tooling window: Complete tooling before the material forms a surface skin, typically about 7 minutes at room temperature and 50% relative humidity.
Cure depth: At room temperature and 50% relative humidity, the sealant cures to a depth of approximately 3 mm in 24 hours. Deep or confined sections and lower humidity extend the cure time.
Illustration of DOWSIL™ 734 Flowable Sealant being applied into a fine joint with an exposed surface for moisture cure

 

Storage, primer, and compatibility

Store at or below 32°C in the original unopened container and keep partially used containers tightly sealed. DOWSIL™ 1200 OS Primer may be used when maximum adhesion is required; allow the applied primer to dry for 15 to 90 minutes at room temperature and at least 50% relative humidity. Adhesion may be limited on PTFE, polyethylene, polypropylene, and related materials. Because the sealant releases a small amount of acetic acid during cure, evaluate corrosion risk on sensitive metals and avoid fully enclosed cure configurations that prevent by-products from escaping.

After cure

Mechanical and electrical properties

Typical values after seven days of cure in air at 25°C and 50% relative humidity unless otherwise stated.

Property Typical value Unit Method / condition
Specific gravity 1.03 — CTM 0022 / ASTM D792
Durometer hardness 27 Shore A CTM 0099 / ASTM D2240
Tensile strength 1.5 MPa CTM 0137A / ASTM D412
Elongation at break 315 % CTM 0137A / ASTM D412
Tear strength, die B 3.0 kN/m CTM 0159A / ASTM D624
Brittle point -65 °C CTM 0057
Dielectric strength 17 kV/mm CTM 0114 / ASTM D149
Volume resistivity 1 × 1015 Ω·cm CTM 0249 / ASTM D257
Permittivity at 100 Hz 2.7 — CTM 0112 / ASTM D150
Permittivity at 100 kHz 2.7 — CTM 0112 / ASTM D150
Dissipation factor at 100 Hz 0.00034 — CTM 0112 / ASTM D150
Dissipation factor at 100 kHz 0.00019 — CTM 0112 / ASTM D150

Elongation is a tensile-specimen property and should not be interpreted as a tested joint-movement classification. Typical values are not intended for use as product specifications.

Applications

Industrial sealing, connector protection, and silicone repair

The flowable consistency is particularly relevant where a conventional non-sag sealant may not readily penetrate a narrow or irregular interface.

Flowable silicone sealant filling a fine joint, crack, or narrow crevice in an industrial assembly
Fine joints and narrow interfaces
The flowable, self-leveling liquid can enter fine joints, cracks, crevices, and small assembly gaps where penetration and uniform coverage are important to the sealing process.
Cable entry and electrical connector interface being sealed with flowable silicone
Cable entries and connectors
Applications include sealing around cable entries and connectors where the liquid must flow around conductors, terminals, or irregular geometries before curing into an electrically insulating silicone rubber.
Field repair of an existing silicone-encapsulated electrical or industrial component
Field repair of silicone gaskets and encapsulants
Its documented adhesion to other silicone rubbers supports repair work where a portion of an existing silicone encapsulant has been removed from installed equipment.
Supporting literature

Product selection resources

DOWSIL™ Silicone Sealants and Foams for Industrial, Appliance and Maintenance
Use this selection guide to compare DOWSIL™ industrial silicone sealant chemistries, cure systems, application characteristics, and related grades. The guide identifies DOWSIL™ 734 as a flowable, self-leveling acetoxy sealant for filling voids, cracks, and crevices.
View selection guide
Certified Solutions for Food and Beverage Processing
This guide provides broader information on Dow silicone solutions for food and beverage processing environments. Use it to review application and certification considerations and verify the exact product, regulatory listing, region, and intended use before selection.
View processing guide
Technical support

Evaluate DOWSIL™ 734 for your sealing or repair application

Krayden can help review joint geometry, substrate preparation, primer requirements, moisture access, cure depth, corrosion-sensitive materials, and electrical property requirements when evaluating DOWSIL™ 734 Flowable Sealant for an industrial assembly or field-repair process.

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel