DOWSIL 895

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

DOWSIL 895

Main features

  • 0 mm Flow/Sag
  • 600% Cured Elongation
  • 15-Minute Working Time

Product Description

DOWSIL 895 Structural Glazing Sealant is a one-part, neutral-cure silicone for structural bonding of glass, metal, and other building components, including attachment of stiffening elements to panels. Typical flow/sag is 0 mm, giving a non-slump application profile. Working time is 15 minutes, and tack-free time is 60 minutes at 50% relative humidity. Typical cured hardness is 38 Shore A. Documented adhesion substrates include glass, anodized aluminum, fluorocarbon-coated aluminum, polyester-powder-coated aluminum or steel, and stainless steel.

Key features

  • Non-slump flow profile: Typical flow/sag is 0 mm for a non-slump application profile.
  • Cured elongation: Typical cured elongation is 600%.
  • Working time: Working time is 15 minutes.

Applications

Structural bonding of glass and metal building components; stiffening-element attachment to building panels.

Technical Specifications

Mechanical Properties
ElongationElongation
600 %
General Properties
Specific GravitySpecific Gravity
1.43
Physical Properties
Tack-Free TimeTack-Free Time
60 minutes
Thermal Properties
Temperature RangeTemperature Range
-50°C to 150 °C

Additional Information

Technical properties

Before-processing sealant properties

PropertyValueUnitMethod / condition
Working time15min
Tack-free time60min50% relative humidity
Flow/sag0mmTypical
Shelf life360daysTypical
Technical properties

Cured sealant properties

PropertyValueUnitMethod / condition
Hardness38Shore ATypical
Elongation600%Typical
Tear strength108.5ppiTypical
Young's modulus145psiTypical

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers