DOWSIL CC-1910
Harmonization Code : 8473.30.80.00 | Parts and accessories (other than covers, carrying cases and the like) suitable for use solely or principally with machines of headings 8470 to 8472 ; Parts and accessories of the machines of heading 8471 ; Other; Other

Main features
- 12,000 mPa s Coating Viscosity
- 13-Minute Tack-Free Time
- UV Indicator for Inspection
Product Description
DOWSIL CC-1910 Conformal Coating is a one-part, translucent silicone conformal coating for printed circuit board assemblies. The no-added-solvent material moisture-cures at room temperature or with heat acceleration and can be needle dispensed. Typical viscosity is 12,000 mPa s, and typical cured hardness is 38 Shore A. A built-in UV indicator provides a visual aid for inspection after application. Documented uses include environmental, corrosion, and dielectric protection of PCBAs and thin-section encapsulation of electronic assemblies.
Key features
- Coating viscosity: Typical viscosity is 12,000 mPa s.
- Humidity-conditioned tack-free time: Tack-free time is 13 minutes at 50% relative humidity.
- UV inspection indicator: A built-in UV indicator provides a visual inspection aid after application.
Applications
Environmental, corrosion, and dielectric protection of PCBAs; thin-section encapsulation of electronic assemblies.
TDS, SDS & Technical Documents
Technical Specifications
Physical Properties
General Properties
Additional Information
Before-processing coating properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Viscosity | 12,000 | mPa s | Typical |
| Tack-free time | 13 | min | 50% relative humidity |
| Solvent added | No | As supplied | |
| Dispense method | Needle |