DOWSIL EG-1200

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

DOWSIL EG-1200

Main features

  • 1:1 Equal-Ratio Mixing
  • 2-Hour Room-Temperature Cure
  • 450 V/mil Dielectric Strength

Product Description

DOWSIL EG-1200 Gel is a two-part, transparent silicone gel with a 1:1 mix ratio for optical coupling and electronics encapsulation. It cures in 2 hours at room temperature or in 60 minutes at 32 deg C, and typical viscosity is 1,790 mPa s. The cured gel has a typical Shore 00 hardness of 51, dielectric strength of 450 V/mil, tensile strength of 43 psi, and thermal conductivity of 0.15 W/(m K). The soft, optically clear material is used for display and LED optical coupling as well as encapsulation, stress relief, electrical insulation, and environmental protection of electronic assemblies.

Key features

  • Equal-ratio gel mixing: The two-part transparent gel uses a 1:1 mix ratio.
  • Dual-temperature cure schedule: Cure time is 2 hours at room temperature or 60 minutes at 32 deg C.
  • Dielectric strength: Typical dielectric strength is 450 V/mil.

Applications

Optical coupling in display and LED assemblies; encapsulation, stress relief, mechanical protection, electrical insulation, and environmental protection of electronics.

Product Family

DOWSIL EG-1200

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
Colorless
Component SystemComponent System
Two (A | B)
Mechanical Properties
ElongationElongation
550 %
Thermal Properties
Temperature RangeTemperature Range
-45°C to 150 °C

Additional Information

Technical properties

Before-processing gel properties

PropertyValueUnitMethod / condition
Mix ratio1:1Two-part system
Viscosity1,790mPa sTypical
Room-temperature cure2hoursRoom-temperature cure
Heat cure60minAt 32 deg C
Technical properties

Cured gel properties

PropertyValueUnitMethod / condition
Durometer51Shore 00Typical
Dielectric strength450V/milTypical
Tensile strength43psiTypical
Thermal conductivity0.15W/(m K)Typical

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers