ECCOBOND 334-1
Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

Main features
- 8-Hour Work Life at 25 deg C
- Moisture Cure in About 1 to 4 Days
- One-Part Tungsten-Filled RTV
Product Description
LOCTITE ECCOBOND 334-1 is a one-part, gray tungsten-filled RTV silicone sealant for room-temperature moisture cure. The material is applied without component mixing and has a typical work life of 8 hours at 25 deg C. Cure typically takes about 1 to 4 days at 25 deg C, depending on relative humidity and bond width. Henkel does not recommend bond lines greater than 1 inch wide because moisture cannot readily reach the center of wider sections. After cure, the material forms a relatively flexible silicone seal for applications where a flexible RTV material is specified.
Key features
- 8-Hour Work Life at 25 deg C: Typical work-life value applies to the one-part RTV silicone before cure.
- About 1 to 4-Day Moisture Cure: The listed cure range applies at 25 deg C.
- Tungsten-Filled RTV Silicone: The gray one-part formulation cures to a flexible material without component mixing.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Work life | 8 | h | 25 deg C; typical |
| Storage life | 122 | days | 25 deg C; continuously dry; typical |
| Cure schedule | 1 to 4 | days | 25 deg C; depends on relative humidity and bond width |