LOCTITE ECCOBOND EO1062

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LOCTITE ECCOBOND EO1062

Main features

  • Low flow
  • Non conductive
  • Excellent reliability

Product Description

LOCTITE ECCOBOND EO 1062 is designed to pass 1,000 hours of temperature/humidity/bias testing and thermal cycling up to 125°C. Exceptional viscosity stability at 25°C provides easier control of shot size using conventional time/pressure dispensing equipment.

 

Cure Schedule

  • 4 to 6 hours @ 125°C - Robust non-stress sensitive components
  • 3 hours @ 140°C.  - Stress sensitive components 
Product Family

ECCOBOND EO1062

1. Select Package Type
2. Select Package Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 50 days
CA Shipping in 12 weeks
EU Shipping in 40 days
Packaging
Please select Package Type and Package Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Pot LifePot Life
600 hours
Specific GravitySpecific Gravity
1.78
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
125 °C
Electrical Properties
Volume ResistivityVolume Resistivity
1.90000000000000 Ohms⋅cm
Physical Properties
ViscosityViscosity
64,000 mPa.s

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers