LOCTITE ECCOBOND FP4802

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

Loctite Eccobond FP4802

Main features

  • High purity
  • Excellent flow
  • Phenolic encapsulant

Product Description

LOCTITE® ECCOBOND FP4802 is a high purity, liquid, phenolic encapsulant designed for use in applications utilizing lead-free solder. This low warpage product can withstand solder reflow temperatures up to 260°C after being exposed to JEDEC level 2 (85°C/60% RH, 168hours) preconditioning. It was formulated to meet “Green” non-halide objectives of many technical users and for temperature cycling ranges up to -65 to 150°C.

LOCTITE ECCOBOND FP4802 features excellent flow properties allowing the material to penetrate fine pitch wires and deep cavities without entrapping voids. A cavity or potting dam is required for flow control.

LOCTITE ECCOBOND FP4802 is suitable for bare chip protection of a variety of advanced packages, such as Ball Grid Arrays (BGA’s), Chip Scale Packages (CSP’s), Plastic Ball Grid Arrays (PBGA’s), and full arrays on Low Temperature cofired Ceramic (LTCC).

 

Cure Schedule

  • 60minutes @ 120°C plus 120minutes @ 165°C
  • 30minutes @ 125°C plus 90minutes @ 165°C

Do not cure with a ramp rate >10°C/minute.

Product Family

ECCOBOND FP4802

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 50 days
CA Shipping in 12 weeks
EU Shipping in 50 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Pot LifePot Life
8 hours
Specific GravitySpecific Gravity
1.76
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
50 °C
Other Properties
MSL LevelMSL Level
MSL 2
Physical Properties
ViscosityViscosity
80,000 mPa.s

Additional Information

LOCTITE ECCOBOND FP4803 is now about to be introduced into the European market. The FP 4803 has been developed for high-volume automotive camera modules and passed all required tests. It claims all the features of 4802 plus a much lower CTE.

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers