Product Description
LOCTITE ECCOBOND UF 1175 partial, white epoxy underfill is formulated for use on large chip sizes, providing good UPH and reliability. Typically used as an electronics encapsulant and a circuit board underfill
LOCTITE ECCOBOND UF 1175 is a fast cure, monocomponent underfill with controlled flow. It offers low CTE and can be dispensed easily and without stringing.
Cure Schedule
- 15 minutes @ 120°C
Packaging
Please select Package Type.
Technical Specifications
General Properties
Specific GravitySpecific Gravity
1.65Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
154 °CPhysical Properties
Thixotropic indexThixotropic index
1.05ViscosityViscosity
35,295 mPa.s