ECCOSORB SF-5.5

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

ECCOSORB SF-5.5

Main features

  • 5.5 GHz Absorber Tuning
  • 163 deg C Maximum Operating Temperature
  • PSA or On-Drawing Options

Product Description

Eccosorb SF-5.5 is a black silicone free-space elastomer microwave absorber grade tuned for 5.5 GHz. It is used on flat or curved metallic surfaces for narrow-band reflectivity reduction and surface-current attenuation. Standard 12X12 NA part 21458167 has a typical density of 3.50 g/cm^3, Shore A hardness of 73, a maximum operating temperature of 163 deg C, and listed reflectivity greater than -20 dB at 5.5 GHz. That standard part measures 305 x 305 mm and 2.33 mm thick. Laird also lists PSA and on-drawing configuration options for the grade.

Key features

  • 5.5 GHz Design Frequency: The grade is tuned for free-space absorption at this frequency.
  • 163 deg C Maximum Operating Temperature: Standard part 21458167 carries this listed operating-temperature limit.
  • About 2.33 mm Standard-Part Thickness: Part 21458167 is supplied as an approximately 305 x 305 mm sheet at this thickness.

Applications

Bonding to flat or curved metallic surfaces for narrow-band microwave reflectivity reduction; radar nacelles; cavity-backed or shrouded telecommunications antennas; surface-current attenuation on metal surfaces; magnetron housings. Not specified for use inside a cavity.

Product Family

ECCOSORB SF-5.5

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Service temperatureService temperature
Max 163 °C
Mechanical Properties
ElongationElongation
20 - 100 %
General Properties
Density (g)Density (g)
2.4-4.5 g/cm3

Additional Information

Technical properties

As-supplied / before-processing properties

Values below apply to standard 12X12 NA part 21458167; other SF-5.5 configurations may differ.

PropertyValueUnitMethod / condition
Density3.50g/cm^3Standard 12X12 NA part 21458167; typical
Hardness73Shore AStandard 12X12 NA part 21458167; typical
Sheet dimensions305 x 305mmStandard 12X12 NA part 21458167
Thickness2.33mmStandard 12X12 NA part 21458167
Technical properties

After-processing / final-state properties

Values below apply to standard 12X12 NA part 21458167; other SF-5.5 configurations may differ.

PropertyValueUnitMethod / condition
Design frequency5.5GHzStandard 12X12 NA part 21458167; typical
Reflectivity>-20dBAt 5.5 GHz; standard 12X12 NA part 21458167; listed value
Maximum operating temperature163deg CStandard 12X12 NA part 21458167

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers