ELANTAS EA-87

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

ELANTAS EA-87

Main features

  • 60 cP Curative Viscosity
  • 50-Minute FR-1046 Gel Time
  • Heat-Required Thin-Film Cure

Product Description

CONACURE EA-87 Hardener is a light-amber epoxy curing-agent component used with selected CONAPOXY resin systems for potting and encapsulation. At 25 deg C, the liquid has a typical viscosity of 60 cP and specific gravity of 1.0. With CONAPOXY FR-1046 Black resin, the system uses 18 parts EA-87 by weight per 100 parts resin and has a 50-minute gel time at 25 deg C; heat is required for cure in thin films. EA-87 is supplied as the standalone hardener component, and these processing and cured-property boundaries apply only to that resin pairing.

Key features

  • Curative Viscosity: EA-87 has a typical viscosity of 60 cP at 25 deg C.
  • FR-1046 Gel Time: The FR-1046 Black/EA-87 system has a typical 50-minute gel time at 25 deg C and uses a 100:18 resin-to-hardener ratio by weight.
  • FR-1046 Thin-Film Cure: Heat is required to cure the FR-1046 Black/EA-87 system in thin films.

Applications

Curing-agent component for selected ELANTAS epoxy potting and encapsulation systems.

Product Family

ELANTAS EA-87

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Liquid
ColorColor
Light Amber
DensityDensity
960 kg/m3
Mix RatioMix Ratio
18
Specific GravitySpecific Gravity
1.0
Thermal Properties
Flash PointFlash Point
>94 °C
Physical Properties
ViscosityViscosity
60 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical EA-87 hardener-component values; the mix ratio shown is specific to CONAPOXY FR-1046 Black resin.

PropertyValueUnitMethod / condition
Viscosity60cPTypical; 25 deg C
Specific gravity1.0-Typical; 25 deg C
ColorLight amber-Typical; as supplied
Mix ratio with FR-1046 Black100:18parts by weightResin:EA-87 hardener
Flash point>94deg CASTM D93

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers