EPOCAP 43648

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

EPOCAP 43648

Main features

  • 10,000 cP Part A Viscosity
  • 100:14 43648/55137 Weight Mix
  • Composite and Electrical Potting Use

Product Description

EPOCAP 43648 Part A is the resin component of the EPOCAP 43648-55137 low-viscosity, two-component epoxy adhesive and laminating system. Part A is a clear amber liquid with typical viscosity of 10,000 cP and specific gravity of 1.16 at 25 deg C. In the paired system, 43648 Part A mixes with 55137 Part B at 100:14 by weight or 8.45:1 by volume. The paired system is used for reinforced-composite assembly, composite fabrication, laminating, and electrical potting. Cured-system values apply only to the 43648/55137 pairing and do not describe Part A alone.

Key features

  • Part A Viscosity: Typical viscosity is 10,000 cP at 25 deg C, with specific gravity of 1.16 for the clear amber resin.
  • 43648/55137 Mix Ratio: The paired system uses 100:14 by weight or 8.45:1 by volume.
  • Composite and Electrical Potting Use: The 43648/55137 system is used for composite assembly, fabrication, laminating, and electrical potting.

Applications

Resin component for the 43648-55137 composite assembly, laminating, and electrical-potting system.

Product Family

EPOCAP 43648

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
Clear Amber
Specific GravitySpecific Gravity
1.16
Physical Properties
ViscosityViscosity
10,000 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Legacy-source typical values for EPOCAP 43648 Part A only.

PropertyValueUnitMethod / condition
ColorClear amber-Legacy source; Part A; as supplied
Viscosity10,000cPLegacy source; Part A; 25 deg C
Weight per gallon9.67lb/galLegacy source; Part A
Specific gravity1.16-Legacy source; Part A; 25 deg C
Shelf life12monthsLegacy source; Part A in a separate sealed container

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers