EPOCAP 45137

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

KALEX 45137

Main features

  • Controlled 100:5.5 Weight Mixing
  • 60-Minute Room-Temperature Gel Window
  • Selected Fuel and Alcohol Resistance

Product Description

EPOCAP 45137/55137 Epoxy Encapsulation System is a two-component, filled epoxy potting material that cures at room temperature for low- to medium-voltage electrical components. The 100:5.5 weight mix ratio produces a red mixed compound with a 60-minute gel time at 25 deg C for a 100 g mass. Vacuum de-airing before and after casting is recommended when the work life permits. After cure, the system provides Shore D 80 hardness, 1.2 W/(m K) thermal conductivity, and high electrical resistivity. Applications include potting and encapsulation of electrical components requiring rigid insulation and resistance to selected fuels and alcohol/fuel mixtures.

Key features

  • Controlled 100:5.5 Mixing: The weight-based mix ratio supports accurate proportioning of the filled resin and hardener.
  • 60-Minute Gel Window: A 100 g mixed mass gels in 60 minutes at 25 deg C.
  • Rigid Electrical Encapsulation: Cured material combines Shore D 80 hardness with high resistivity and dielectric strength.

Applications / Suitable for

  • Low- to medium-voltage electrical component potting
  • Electrical encapsulation and insulation
  • Cast assemblies exposed to selected fuels and alcohol/fuel mixtures
Product Family

EPOCAP 45137

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Service temperatureService temperature
105 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical component, mixed-system, and processing properties before final cure.

Property Value Unit Method / condition
Mix ratio by weight 100:5.5 45137 resin to 55137 hardener
Mix ratio by volume 100:9 45137 resin to 55137 hardener
Part A viscosity 12,000 cps 45137 resin at 25 deg C
Part B viscosity 40 cps 55137 hardener at 25 deg C
Mixed specific gravity 1.58 At 25 deg C
Gel time 60 minutes 100 g mass at 25 deg C
Shelf life 12 months Each component in a separate sealed container
Storage temperature 16 to 27 deg C Dry environment
Technical properties

After-processing / final-state properties

Typical cured properties after the stated room-temperature or accelerated cure schedule.

Property Value Unit Method / condition
Hardness 80 Shore D Cured material; tested at 25 deg C
Tensile strength 7,968 psi Cured material; tested at 25 deg C
Compressive strength 12,030 psi Cured material; tested at 25 deg C
Flexural strength 15,280 psi Cured material; tested at 25 deg C
Elongation 0.84 % Cured material; tested at 25 deg C
Thermal conductivity 1.2 W/(m K) Cured material
Volume resistivity 1.06 x 10^15 ohm cm Cured material at 25 deg C
Dielectric strength 358 V/mil Cured material at 1/8 inch thickness

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers