EPOCAP 59174
Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

Main features
- 500 cP Part B Viscosity
- 100:30 49174/59174 Weight Mix
- Electrical Potting and Impregnation
Product Description
EPOCAP 59174 Part B is the amber hardener supplied as Part B for the EPOCAP 49174/59174 epoxy encapsulation system. At 25 deg C, Part B has a typical viscosity of 500 cP and specific gravity of 0.96. It pairs with black 49174 Part A at 30 parts hardener per 100 parts resin by weight, or 50 parts per 100 by volume. After mixing, the low-viscosity electrical potting system is used for impregnation of coils, transformers, time-delay relays, and other low- or medium-voltage assemblies. Final cured performance applies to the complete 49174/59174 system rather than Part B alone.
Key features
- Part B Viscosity: Typical viscosity is 500 cP at 25 deg C, with specific gravity of 0.96 for the amber hardener.
- 49174/59174 Mix Ratio: The paired system uses 100:30 by weight or 100:50 by volume.
- Electrical Potting and Impregnation: The complete paired system is used for coils, transformers, time-delay relays, and related assemblies.
Applications
Part B hardener for the 49174/59174 electrical potting and encapsulation system used with tightly wound coils, transformers, time-delay relays, and related devices.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Additional Information
As-supplied / before-processing properties
Legacy-source typical values for EPOCAP 59174 Part B only.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Color | Amber | - | Legacy source; Part B; as supplied |
| Viscosity | 500 | cP | Legacy source; Part B; 25 deg C |
| Weight per gallon | 8 | lb/gal | Legacy source; Part B |
| Specific gravity | 0.96 | - | Legacy source; Part B; 25 deg C |
| Filler type | None | - | Legacy source; Part B |
| Shelf life | 12 | months | Legacy source; Part B in a separate sealed container |