EPOCAST 1615

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

EPOCAST 1615

Main features

  • 0.70 g/cc Mixed Density
  • 15-Minute Gel Time
  • Self-Extinguishing Cured System

Product Description

EPOCAST 1615 A/B is a two-component, low-density epoxy syntactic edge sealant for honeycomb structures. The off-white Part A and amber Part B mix at 100:14 by weight to form an off-white paste with typical density of 0.70 g/cc and a 15-minute gel time at 25 deg C. The system cures in 24 hours at 25 deg C, or after room-temperature gel followed by five hours at 52 deg C. The system combines flame resistance and high strength with qualification to BMS 5-28, Type 15 for aerospace composite edge sealing.

Key features

  • 0.70 g/cc Mixed Density: The off-white mixed paste is used for honeycomb edge-seal applications.
  • 15-Minute Gel Time: This typical value applies to a 50 g mass at 25 deg C.
  • Self-Extinguishing Flammability: Horizontal and vertical flammability results are self-extinguishing for the cured system.

Applications

Honeycomb core edge sealing; aerospace composite structures.

Product Family

EPOCAST 1615

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
Off-white
DensityDensity
700 kg/m3

Additional Information

Technical properties

As-supplied / before-processing properties

Typical Part A, Part B, and mixed-system properties from the exact Huntsman TDS.

PropertyValueUnitMethod / condition
ColorOff-white / amber / off-white-Part A / Part B / mixed system; visual
Density0.65 / 1.05 / 0.70g/ccPart A / Part B / mixed system; ASTM D1622
ViscosityPaste / 400 / pastecPPart A / Part B / mixed system; 25 deg C; ASTM D2196
Gel time15minutesMixed system; 50 g at 25 deg C; ASTM D2471
Mix ratio100:14parts by weightPart A resin:Part B hardener
Technical properties

After-processing / final-state properties

Typical cured-system values; cure schedule is 24 hours at 25 deg C or room-temperature gel plus 5 hours at 52 deg C.

PropertyValueUnitMethod / condition
Tensile lap shear700psiAfter 5 hours at 52 deg C; ASTM D1002
Compressive strength6.0KsiAt 25 deg C; ASTM D695
Compressive modulus450KsiAt 25 deg C
Horizontal flammabilitySelf-extinguishing-Typical cured-system result
Vertical flammabilitySelf-extinguishing-Typical cured-system result
Maximum flow at 25 deg C1.0in.Typical cured-system result

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers