EPOXYLITE E230

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

EPOXYLITE E230

Main features

  • Low-Temperature Trickle Impregnation
  • 15 to 25 Minute Gel Time
  • 1,700 Volts/Mil Dielectric Strength

Product Description

EPOXYLITE E230 is a two-component, low-temperature-curing, 100%-solids epoxy impregnating-resin system used with EPOXYLITE C230 hardener. The components mix at 100:20 by weight or 100:22.6 by volume. At 25 deg C, the mixed resin has typical viscosity of 3,000 to 6,000 cP and a 15 to 25 minute gel time for a 250 g mass. Application methods include trickle and brush-on processing for motor and transformer windings, high-speed armatures, and protective overcoating.

Key features

  • Low-Temperature Trickle Impregnation: The system is used for trickle application into motor and transformer windings.
  • 15 to 25 Minute Gel Time: This typical range applies to a 250 g mixed mass at 25 deg C.
  • 1,700 Volts/Mil Dielectric Strength: Typical cured properties also include 1.1 x 10^15 ohm-cm volume resistivity.

Applications

Motor and transformer winding impregnation; high-speed armatures; protective overcoating of motor windings; appliance motors.

Product Family

EPOXYLITE E230

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Component SystemComponent System
Two Part (Resin | Hardener)
Chemical Properties
Water AbsorptionWater Absorption
0.2 %
Electrical Properties
Dielectric StrengthDielectric Strength
66.93 kV/mm
Volume ResistivityVolume Resistivity
1.1 x 10¹⁵ Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical E230 resin, C230 hardener, and mixed-system values from the exact ELANTAS TDS.

PropertyValueUnitMethod / condition
Resin viscosity10,000 to 15,000cPE230 resin; 25 deg C
Hardener viscosity100 to 500cPC230 hardener; 25 deg C
Resin weight per gallon9.5 to 9.9lbE230 resin; 25 deg C
Hardener weight per gallon8.4 to 8.8lbC230 hardener; 25 deg C
Mix ratio100:20parts by weightE230 resin:C230 hardener
Mix ratio100:22.6parts by volumeE230 resin:C230 hardener
Mixed viscosity3,000 to 6,000cP25 deg C
Gel time15 to 25minutes250 g mixed mass at 25 deg C
Technical properties

After-processing / final-state properties

Typical cured-system values; process and cure conditions must be selected from the exact TDS for the intended unit and application.

PropertyValueUnitMethod / condition
Helical-coil bond strength40lbAt 25 deg C; ASTM D2519 over MW 35
Helical-coil bond strength4lbAt 150 deg C; ASTM D2519 over MW 35
HardnessShore D 75 to 85-Typical cured-system value
Water absorption0.2%24 hours at 25 deg C
Dielectric strength1,700volts/mil25 deg C; 3 mils; ASTM D149
Volume resistivity1.1 x 10^15ohm-cm25 deg C; ASTM D257
Dielectric constant3.8-1 kHz at 25 deg C
Dissipation factor0.03-1 kHz at 25 deg C

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers